The core polymer particles in an elastomer emulsion, providing elasticity and strength.
| Parameter | Typical range | Notes & selection driver |
|---|---|---|
| Particle Size | 0.1-1 μm | |
| Solids Content | 40-60% | |
| Mooney Viscosity | 30-60 ML(1+4)100°C | |
| Glass Transition Temperature | -50°C to -20°C |
Ranges are indicative industry figures for RFQ preparation, not a supplier commitment. Confirm every value and standard with the legal manufacturer before ordering.
This component is used in the following industrial products
A practical evidence checklist for RFQ preparation and supplier evaluation.
CNFX does not score or rank suppliers. Buyers must verify all claims and documents with the legal manufacturer before ordering.
Manufacturer profiles associated with Elastomer Polymer Particles.
Manufacturer listings support early research and capability understanding. They are not certification, ranking, or transaction guarantees.
A smaller particle size increases the specific surface area, which raises crosslink density and strength, but can reduce flow during processing.
Store them in a cool, dry place out of direct sunlight, below 30 °C and below 60 % relative humidity.